Follow us :

  • A: If you bond the glass with other parts fully by optical bonding, the gloss will vary,the gloss of double side AG glass will increase by 10-20. If it’s single side AG glass or bonded half, the gloss varies small.

  • A: If you bond the glass with other parts fully by optical bonding, the gloss will vary,the gloss of double side AG glass will increase by 10-20. If it’s single side AG glass or bonded half, the gloss varies small.

  • A: FELIX GLASS AG glass is immersed etching. Technically speaking, we have to cover another side when we’re etching single side AG glass.

  • A: For custom gorilla glass, gorilla glass 3, gorilla glass 4 and anti glare glass. FELIX GLASS provide CNC machining,chemical strengthening,multi-color printing, AF coating, AR coating, anti glare etching and double side 3M tape service. A. CNC machines to process any desired shape. Chamfer / Bevel/Holes etc. B.Chemical strengthening to make glass stronger and tougher, with best performance of an...

  • A: Dimension: ±0.05mm ( 5”) Printing: ±0.1mm 16.How many days to deliver custom anti glare glass ? For custom anti glare glass, single side etching and double side etching. FELIX GLASS import high quality raw material abroad, the applicable kinds are very wide. The lead time depends on the current stock, please kindly contact sales.

  • A: 100pcs-1000pcs. We will provide you 10pcs samples in prototype stage

  • A: To ensure the quality of custom gorilla glass and anti glare glass. We will make full inspection after every procedure, IPQC and make spot check before delivery. ISO9001:2008 quality management system is strictly carried out.

  • A: No matter it’s single side AG glass or double sided AG glass, both can be silkscreen printed.

  • A: Haze refers to percentage of incident transmission light which deviates more than 2.5°accounts for total incident transmission light, the unit symbol is %. The higher the haze is, the lower the gloss and the resolution is.

  • A: The production information of gorilla glass (2320) and 4(5318)are enclosed. Please download for your reference.

  • A: Gorilla glass 3, gorilla glass 4, gorilla glass 2320. Above 90% samples are delivered within 7 days. For mass production, it’s always 15days

  • A: The easiest way is to hold the AG glass under a fluorescent light and look at the tube reflected on the glass from the front. If the light is scattered on the glass, it is etched side. If the light is clearly visible, it is a non-ag side. This is the most direct way to distinguish from the visual effect.

  • A: FELIX GLASS Standard Water Contact Angle is 105°, Abrasion Test: 200g weight,Steel Wool#0000, 2000times(back and forth as 1 time),Recession Value within 15%​​

  • A: Definitely not. Because the etched glass surface is only about 0.05mm depth, and the chemical strengthening is immersion type, which can fully complete the replacement of ions. We have done too many time tests and the results showed that it didn’t affect the strength of the glass.

  • A: This question has written a lot of introduction, You can search on the FELIX GLASS website and you will find related videos, introductions, and pictures. “Dead Fronteffect”(All-in-one-black), that is to say, the display is clearly visible when back-lit, and when non-backlit, the entire display including glass is completely black without a color difference. Dead front glass is widely used in sma...

  • A: Corning Gorilla Glass Stress Value: DOL40um, CS650Mpa Soda Lime Glass Stress Value: DOL8um, CS450Mpa ​

  • A: ①Printing, suitable for small area printing within 20*20mm. ②Electroplating, suitable for small sizes below 7 inches ③The glass material is gray glass, and the maximum size can be 32 inches. ④Film Adhesion, unlimited size

  • A: AG, AR and AF can be realized on the same cover glass, which is called 3A. It is standard for display cover glass.