AR anti-reflection
Reduces surface reflection and supports display readability. The source lists up to 97% light transmittance for an AR-coated configuration.





US $8.115 - 99 piece
US $6.98100 - 999 piece
US $5.891000 - 4999 piece
US $2.885000 - 9999 piece
Paramtents
Substrate Ultra-low iron industrial tempered glassUltra-low iron industrial tempered glass
Available Coatings AR / AR+AF / AG+AF / AR+AF+AG
Light Transmittance ≥92% (97% for AR coating)
AG Haze Range 5%–15% adjustable
AF Water Contact Angle ≥110°
Surface Hardness 9H Mohs scratch resistance
Thickness Options 1.1mm / 2.0mm / 3.0mm / 5.0mm
Working Temperature -40℃ ~ 180℃
Custom Processing CNC cutting, drilling, full edge chamfering, black border silk printing
Compliance ISO 9001, RoHS, REACH
Packging & Delivery
Min Order5 piece
Briefing
Detailed
Felix Glass manufactures tempered optical cover glass for industrial HMI control panels, factory touchscreens, CNC equipment, PLC terminals, outdoor industrial displays, warehouse monitoring systems, and test instruments.
The source product describes ultra-low-iron tempered glass with magnetron-sputtered optical coatings and drawing-based machining. AR anti-reflection, AF anti-fingerprint, and AG anti-glare functions can be specified separately or in combinations.
This product remains in the Industrial Touch Panel Glass category.
The values below retain the source product specification. Final substrate, coating stack, dimensions, optical targets, durability, and compliance documents must be confirmed for the selected configuration.
Each surface treatment addresses a different interface condition and should be defined with measurable acceptance criteria.
Reduces surface reflection and supports display readability. The source lists up to 97% light transmittance for an AR-coated configuration.
A hydrophobic and oleophobic surface reduces oil, dust, and fingerprint adhesion and supports routine cleaning.
A matte surface diffuses reflected workshop light. The source lists an adjustable haze range of 5%–15%.
Browse other touch and display solutions in the Felix Glass product catalog.
These are starting points, not fixed prescriptions. Haze, sparkle, sharpness, reflectivity, touch behavior, cleaning, and cost should be evaluated on the actual display stack. Learn more about the company on About Us.
| Substrate | Ultra-low-iron industrial tempered glass |
|---|---|
| Coatings | AR, AR+AF, AG+AF, or AR+AF+AG |
| Light transmittance | At least 92%; 97% reference for AR-coated glass |
| AG haze | 5%–15% adjustable reference |
| AF water contact angle | At least 110 degrees reference |
| Surface hardness | 9H scratch-resistance reference |
| Thickness options | 1.1, 2.0, 3.0, and 5.0 mm |
| Working-temperature reference | -40°C to 180°C |
| Custom processing | CNC cutting, drilling, edge chamfering, and black-border silk-screen printing |
| Compliance references | ISO 9001, RoHS, and REACH |
The temperature range and compliance references require project-specific verification. Request the test method, component scope, certificate, issuing organization, and validity period before relying on them.
Additional coating and display guidance is available in the Felix Glass blog.
The source identifies the following application groups. Each installation should be reviewed for lighting, touch stack, cleaning, temperature, vibration, ingress protection, and operator use.
The source lists custom size, thickness, irregular profiles, CNC openings, notches, chamfers, black borders, logos, and positioning marks. Prototype and volume programs can be discussed after the process route is reviewed.
Start from the Felix Glass home page for a broader view of material and processing capabilities.
The original description states that hardness, transmittance, and surface quality are inspected before delivery and that optical test reports can be provided. It also references a stable coating line, engineering support, sampling, and international delivery.
For supplier qualification, define the sampling plan, traceability, appearance limits, optical methods, hardness method, coating-wear test, packaging, sample lead time, production capacity, and shipment terms. Statements about fast sampling or stable delivery should be confirmed in the order schedule.
The source recommends AR+AF as a starting point for display readability and cleaning. The final choice depends on lighting, display brightness, touch frequency, and cost.
The source states that the sputtered coatings support routine cleaning. Validation must use the actual oil, cleaner, cloth, load, cycle count, and acceptance criteria.
The source lists 9H. The purchase specification should identify the hardness scale, method, load, sample condition, and pass criteria.
Yes, subject to CAD review, glass thickness, openings, edge distance, print artwork, tolerances, and inspection requirements.
Use Contact Us to request project-specific test data and documentation.
The original description contained unverified placeholders for touch cover glass, quartz glass, ITO, and FTO products. Those placeholders are removed. Use the approved product catalog and blog paths above to compare cover-glass substrates, conductive glass, coating combinations, and processing options.
Send the HMI drawing, substrate, thickness, coating combination, target haze, transmittance and reflectivity, openings, edge geometry, printing artwork, cleaning chemicals, environment tests, compliance documents, sample quantity, annual volume, and requested schedule.
网络文化经营许可证:浙网文[2013]0268-027号|增值电信业务经营许可证:浙B2-20080224-1 2007-2026 Tradevv.com. All rights reserved.